Pourbles / Fixes / Cracking and crazing

Why is my pour cracking?

Cracks appear when the top of the paint dries and shrinks before the paint underneath has caught up. Fine, spidery surface cracks are usually called crazing; wider cracks can go right down to the canvas. The causes overlap.

1. The paint layer is too thick

Pours put down far more paint than brushwork, and a thick layer takes a long time to dry right through. The surface skins over first; as the wet paint underneath keeps drying and shrinking, it pulls the skin apart. Puddles in a dip in the canvas are the usual place for cracks.

Try: use the amount you need rather than extra on the canvas (the paint amount calculator helps), tilt so the paint spreads to an even depth, and make sure the canvas is level and not sagging in the middle. Tightening or propping a saggy canvas from underneath stops paint pooling.

2. It dried too fast

Warm, dry or moving air dries the surface faster, which makes the skin-then-shrink problem worse. Heaters, fans, air conditioning blowing across the table, and direct sun are common culprits.

Try: dry pours flat in a still, room-temperature spot, away from vents and sun, and give them time. Covering the painting loosely with a big box (not touching it) keeps dust off and slows the surface down.

3. Too much water

Water thins the paint, but it also dilutes the binder that holds dry paint together. Paint thinned mostly with water is weaker and more likely to crack.

Try: thin with pouring medium and use water only for the last small adjustment.

4. A glue-heavy or mismatched medium

Glue and water mixes, and some other cheap mediums, are more prone to crazing than purpose-made pouring mediums, especially in thick layers. Mixing very different paints and mediums in one pour can also make layers dry at different speeds.

Try: if crazing keeps happening with a glue mix, try a commercial pouring medium for comparison, or keep glue pours thin.

5. Low-binder paint

Some very cheap craft paints carry a lot of filler and relatively little binder, and can crack more readily when poured thick.

Try: if one particular colour always cracks, try a different brand of that colour.

Can I fix cracks once they've happened?

Fine crazing on a dry pour can often be hidden with a coat of gloss varnish or a resin coat, which fills the surface. Wide cracks that reach the canvas are harder: you can pour a fresh layer over the top once the old one is fully dry, or treat the cracks as part of the piece. Some pourers like the look.

A quick checklist

CheckWhat to aim for
LayerEven depth, no puddles, canvas level and not sagging
DryingFlat, still, room temperature, out of the sun
WaterA little, last, only for fine-tuning
MediumA purpose-made pouring medium if glue mixes keep crazing

Supplies mentioned here

Written from widely shared pouring practice; see also artsupplies.co.uk, common acrylic paint pouring problems. Last checked 27 November 2026.